Deoxidation iron requirements of seamless steel pipe ...
Density: Deoxidation iron from the roof into the furnace, must be able to pass through the slag layer, to stay in the slag / steel liquid interface, so you can ensure efficient heat transfer and chemical reactions. If Deoxidation iron density is too low, it will float on the surface of the slag; and high density of the liquid steel will wear to go.